The reduction of the critical conditions and the particle-promoted nucleation mechanism work together to increase the amount of dynamic recrystallization. In addition, it was found that alloys with 6 wt.% Zn elements tend to undergo a dynamic recrystallization softening mechanism, while alloys with 3 wt.% Zn elements tend to undergo a dynamic reversion softening mechanism.Grain size is one of the most important parameters for metallographic microstructure analysis, which can partly determine the material performance. The measurement of grain size is based o