Their IPA, which determines their network structure, was modulated by varying the feed concentration of the neutral monomer, Cnm. An increase of Cnm within an optimized Cnm window (0.3-0.4 M) decreased the cross-linking density (strength and density of the IPAs) of the PAT hydrogels, reducing the softening temperature and Young's modulus, which increased compliance but maintained sufficient mechanical strength and thereby maximized the contact surface and enhanced skin adhesion. The DMAAm monomers, compared to the HEMA monomers, produced