https://pi-3065inhibitor.com/f....rom-natrual-envirome
We discovered the slip of SS cable through the dies was essential for the graphite finish in terms of running amount and stability. Once the graphite coated SS wire had been prepared once the anode and operated in a BESs, the existing thickness reached 1.761 ± 0.231 mA cm-2, that was 20 times higher than that without graphite coating. Biomass analysis ended up being conducted, guaranteeing the superior bioelectrochemical performance was attributed to the improvement of biocompatibility