Micro-/nano-structured scaffolds with a weight composition of 46.6% α-tricalcium phosphate (α-TCP)-53.4% silicocarnotite (SC) were synthesized by the polymer replica method. The scanning electron microscopy (SEM) analysis of the scaffolds and natural cancellous bone was performed for comparison purposes. Scaffolds were obtained at three cooling rates via the eutectoid temperature (50 °C/h, 16.5 °C/h, 5.5 °C/h), which allowed the surface nanostructure and mechanical strength to be controlled. Surface nanostructures were characterized by transmissio