https://www.selleckchem.com/CDK.html
The weld joints of sprayed 2195-T6 and cast 2195-T8 aluminium-lithium alloy were created using tungsten inert gas with filler wire. The microstructures and mechanical properties of the weld joints were examined. The results of the microstructure analysis showed that the width of the equiaxed grain zone (EQZ) and the amount of the second phase θ'(Al2Cu) was greater in the weld joint of the cast 2195-T8 Al-Li alloy than that of the sprayed 2195-T6 Al-Li alloy. Tensile testing indicated that failures occurred in the EQZ and partially melted zone (PMZ)