7 MP) followed by conventional adhesive/silane (11.9 MP), conventional adhesive without silane (7.6 MP), and universal adhesive without silane (4.4 MP). In the absence of silane, the conventional adhesive yielded significantly higher SBS than universal adhesive (P = 0.03). In the presence of silane, the two adhesives showed SBS values significantly higher than the values obtained when silane was not applied, while the two adhesives were not significantly different in terms of SBS in the presence of silane (P = 0.53). Based on ARI score,