Film thickness varied largely among materials. All preheated resin composites had films thicker than 50 μm without ultrasound energy. Application of ultrasound reduced film thickness between 21% and 49%. Linear and nonlinear regressions did not identify any relationship between filler loading, viscosity, and/or film thickness. All materials showed quick temperature reduction following preheating, showing maximum temperature loss rates after approximately 10 s. Distinct restorative resin composites react differently to preheating, affect