Atomic layer deposition (ALD) is a promising deposition method to precisely control the thickness and metal composition of oxide semiconductors, making them attractive materials for use in thin-film transistors because of their high mobility and stability. However, multicomponent deposition using ALD is difficult to control without understanding the growth mechanisms of the precursors and reactants. Thus, the adsorption and surface reactivity of various precursors must be investigated. In this study, InGaO (IGO) semiconductors were depo