The CrFeCoNiNb0.3Mo0.3 alloy had the smallest corrosion rate (0.0732 mm/yr) in 1 M deaerated H2SO4 solution, and the CrFeCoNiNb0.15Mo0.15 alloy had the smallest corrosion rate (0.0425 mm/yr) in 1 M deaerated NaCl solution. However, the CrFeCoNiNb0.5Mo0.5 alloy still had the best combination of corrosion resistance and hardness in the present study.Up to now, 12 μm thick rolled copper foil is the thinnest rolled copper foil that can be stably produced. The softened microstructure and properties of 12 μm thick rolled copper foil were