Statistical analysis was done using one-way ANOVA test and Kruskal-Wallis test (α=.05). The group repaired with bis-acryl composite without additional surface treatment showed the highest mean shear bond strength. It was significantly higher than all four groups repaired with methylmethacrylate ( .05). Additional surface treatments, neither mechanical nor chemical, increased the shear bond strength within methylmethacrylate groups and bis-acryl composite groups ( .05). Failure mode analysis showed that cohesive failure was