https://www.selleckchem.com/products/cm-4620.html
The addition of TU led to properties that were similar or worse than the materials to which it was not added, except for dimensional stability. The impact on properties was statistically significant for all materials above 20% addition of TU. The addition of DMAM at 5 wt% or isobornyl methacrylate at 10 wt% improved yield strength and modulus, but increased water sorption and solubility. Except for dimensional stability, the addition of thiourethane oligomers to acrylic denture base materials compromised most tested properties. The use