https://www.selleckchem.com/products/tram-34.html
The lowest value of 2 h water absorption rate (3.3% ± 0.3%) and thickness swelling rate (2.2% ± 0.4%) of composite were obtained when the SA concentration was 0.15 M. In addition, the introduction of SA can not only enhance the water resistance of the composite laminates, but also reduce the loss of tensile strength in wet conditions, which shows potential in outdoor applications.Objectives were to investigate somatic cell counts (SCC) and total bacterial counts (TBC) in the raw bulk-tank milk of sheep flocks in Greece, to study factors