https://www.selleckchem.com/pr....oducts/gmx1778-chs82
Atomic layer deposition (ALD) is a highly controllable thin film synthesis approach with applications in computing, energy, and separations. The flexibility of ALD means that it can access a massive chemical catalogue; however, this chemical and process diversity results in significant challenges in determining processing parameters that result in stable and uniform film growth with minimal precursor consumption. In situ measurements of the ALD growth per cycle (GPC) can accelerate process development but it still requires expert