The objective of this study was to assess the influence of alumina sandblasting on the flexural strength of the latest generation of highly translucent yttria partially stabilized dental zirconia (Y-PSZ). Fully-sintered zirconia disk-shaped specimens (14.5-mm diameter; 1.2-mm thickness) of four Y-PSZ zirconia grades (KATANA HT, KATANA STML, KATANA UTML, all Kuraray Noritake; and Zpex Smile, Tosoh) were sandblasted at 0.2 MPa with 50-μm alumina (Al2O3) sand (Kulzer) or left as-sintered (control). For each zirconia grade, the yttria (Y