The 800 ℃ heat treatment shows a powerful oxide layer which increases layer crystallinity from 64per cent to 75per cent and layer glue relationship strength from 25.9 ± 2.3 MPa to 30.7 ± 1.1 MPa, while simultaneously reducing the dissolution price of HA coatings. The inclusion of biologically relevant dopants, MgO and SiO2, show minimal effects on crystallinity and adhesive relationship power on plasma-sprayed HA coatings, but, in vitro evaluations show an enhancement effect on osteobla