During welding of glass with ultrafast lasers, an irregular formation of weld seams was prevented by modulation of the average laser power and spatial beam shaping. The formation of individual molten volumes in regular intervals was achieved by means of power modulation, resulting in a predictable and reproducible weld seam with a regular structure. At constant average power, a homogeneous weld seam without a periodic signature was alternatively achieved by means of a shaped beam generating an elongated interaction volume and