63 J cm-3 at an enhanced breakdown strength of 480 MV m-1. This obtained high discharge energy density is 84% higher than the pure PVDF film and 582% higher than a commercialized biaxially oriented polypropylene (BOPP). Large interfacial polarization and strong interaction of polymer chains between the PVDF polymer and P(VDF-TrFE-CFE) terpolymer may contribute to the tunable dielectric constant and electric breakdown strength, thus promoting the energy storage capability. This work establishes a facile, but effective approach to achiev