https://www.selleckchem.com/products/ga-017.html
RESULTS Under baseline conditions, all groups presented similar bond strengths, but only SiC and 7% Si yielded unaltered bond strength after aging. SiC and 7% Si presented lower contact angles. All groups presented similar surface topographies. The silica content was also similar among groups, except for AlOx. CONCLUSION 7% Si and SiC presented similar bond strength and better bonding performance after aging than AlOx and 20% Si. A higher silica concentration was not able to promote stable adhesion of composite cement after aging.PURPOSE