https://www.selleckchem.com/pr....oducts/bgb-3245-brim
The effects of reactor temperature and shear force were evaluated, with the finding that reactor temperature can minimize the catalyst-cellulose interaction barrier, promoting coagulation, but that the shear force in a typical laboratory reactor cannot. We have evaluated strategies for enhancing cellulose-catalyst interaction and conclude that raising reaction temperature or synthesizing acid/base bifunctional catalysts can effectively diminish electrostatic repulsion and promote cellulose-catalyst coagulation. The analysi