This study focuses on the energy potential and combustion process of torrefied wood. Samples were prepared through the torrefaction of five types of wood Ash, beech, oak, pine and spruce. These were heated for 2 h at a temperature of 300 °C under a nitrogen atmosphere. Torrefied wood was prepared from wood samples with dimensions of 100 × 100 × 20 mm3. These dimensions have enabled investigation of torrefied wood combustion in compact form. The effect of the external heat flux on the combustion of the samples was measured using a cone calorimeter. T