Yttria doped ZrO2 was deposited using an acidic zinc phosphatizing solution and the hydrothermal treatment. The coating was analyzed using a field emission-scanning electron microscope (FE-SEM), X-ray diffraction (XRD), energy-dispersive X-ray spectroscopy (EDX) and X-ray photoelectron spectroscopy (XPS). A piston on three balls (ISO 6872) was used for the measurement of biaxial flexural strength. MC3T3-E1 cells attachment was evaluated by SEM, and cell proliferation were assessed using MTS assay™. SEM images confirmed that the zinc pho