The maximum SBS was displayed in group 1, dentin conditioned with ECL and bonded to C (20.23 ± 0.47 MPa). Whereas, group 6, PDT of dentin to BA demonstrated lowest bond integrity among experimental groups (12.97 ± 0.25 MPa). Bond strength of group 1, ECL-C (21.55 ± 3.08 MPa) and group 3 EYL-C (19.11 ± 0.65 MPa) were comparable (p  0.05). Group 5 samples treated with PDT, MB-C (13.41±0.32 MPa) and group 6, MB-BA (12.97 ± 0.25 MPa) were also comparable (p  0.05) CONCLUSION BAc bonded to dentin after surface conditioning with ECL,