While, addition of larger mass fractions (7.5 and 10 wt. %) of the HNT/Ag did not show further improvement in the mechanical properties of dental resins composites. Theses composites also demonstrated satisfactory depth of cure and degree of conversion. A significant antibacterial activity was observed on S. mutans. No significant cytotoxicity was found on NIH-3T3 cell lines. Conclusion The incorporation of HNT/Ag in Bis-GMA/TEGDMA dental resins composites resulted in enhancement in mechanical as well as biological properties for dental ap