Carbon nitride materials require high temperatures (500 °C) for their preparation, which entails substantial energy consumption. Furthermore, the high reaction temperature limits the materials' processability and the control over their elemental composition. Therefore, alternative synthetic pathways that operate under milder conditions are still very much sought after. In this work, we prepared semiconductive carbon nitride (CN) polymers at low temperatures (300 °C) by carrying out the thermal condensation of triaminopyri