https://www.selleckchem.com/mTOR.html
The resulting significant microwave absorptions reveal that our g-C3N4/NiCo2S4/PVDF 40% nanocomposite exhibited seven notches of reflection loss (RL), more than 30 dB in its curve, at 1.75 mm in thickness, while its maximum RL was 59.39 dB at 13.07 GHz. Interestingly, this composite, in a mass fraction of 60%, illustrates an efficient bandwidth of 5.1 GHz (RL 10 d at only 1 mm thickness. It is worth noting that the maximum RL of g-C3N4 stick structures/PVDF measures 74.53 dB at 14.86 GHz, with a broadband efficient bandwidth of 7.96 GHz (RL