Thermal conductivity and density increased in all groups containing AuNps compared to the control group, but it was not significant in all groups. Vickers hardness values increased significantly with an increase in AuNps` content, with the highest value 21.45 HV obtained at 0.74 wt% of AuNps. Statistical analysis was performed by means of the SPSS 19 software package. Incorporation of AuNps into heat-polymerised PMMA resin led to decrease of the flexural strength and elastic modulus. At the same time, the density, thermal con