https://mtor-signal.com/preper....itoneal-insufflation
The in-situ atomic force microscopy results suggested that the decomposition response occurred in the ethylene carbonate-based electrolyte solution at a possible of ~0.68 V, as the lithium alloying response happened below 0.25 V during the very first reduction procedure. The decomposition response was more vigorous and took place at a greater potential in the propylene carbonate-based electrolyte solution, leading to the synthesis of a thick solid electrolyte interphase film