The efficiency of material removal by electrochemical machining (ECM) and rim zone modifications is highly dependent on material composition, the chemical surface condition at the break through potential, the electrolyte, the machining parameters and the resulting current densities and local current density distribution at the surfaces. The ECM process is mechanistically determined by transpassive anodic metal dissolution and layer formation at high voltages and specific electrolytic compositions. The mechanisms of transpassive anodic metal dissolut